MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
ChevronTexaco Pinnacle® EP 1000
Categories: Fluid; Lubricant

Material Notes: Texaco Pinnacle EP oils deliver value through:
  • Excellent thermal and oxidation stability — The synthetic hydrocarbon base oils used in these products provide outstanding stability resulting in longer lubricant and equipment life.
  • High viscosity index and low pour point — These result in very broad operating temperature ranges -46°C to 149°C (-50°F to 300°F) when compared with conventional mineral oil based lubricants.
  • Energy savings — The synthetic base oil will typically increase gear efficiency, resulting in less power consumption.
  • Extended drain intervals — Longer lubricant life, reduced maintenance costs, and less used oil disposal when compared to mineral oil products.

Texaco Pinnacle EP oils are high quality industrial EP gear lubricants.

They provide excellent load carrying and antiwear properties; protection against rust, corrosion, foaming, and oxidation; and excellent demulsibility resulting in high performance in most types of industrial gearboxes, exemplified by the FZG pass stage of >12.

These products possess very high shear stability even under heavily loaded, high speed conditions in industrial gears.

The low pour point and very good low temperature fluidity of Texaco Pinnacle EP oils impart improved lubrication during startup at sub-zero temperatures.

Their superior viscosity-temperature characteristics provide dependable lubrication at high temperatures.

A unique property of the synthetic base oil is a low traction coefficient, resulting in improved gear efficiency, energy savings, less friction, less wear, and lower operating temperatures compared to conventional mineral oil products.

Due to the very high viscosity index, these products provide a much higher oil viscosity at operating temperature than a mineral oil product of the same ISO grade. This results in increased oil film thickness and better antiwear protection for both bearings and gears.

Texaco Pinnacle EP oils are recommended for all types of enclosed industrial gearboxes:

  • Especially those running continuously at temperatures up to 107°C(225°F)
  • Or exposed to very cold temperatures as low as -46°C(-50°F)
  • Or under severe service conditions, such as heavy loads or low speeds.

These products also provide excellent protection for bearings operating under similar conditions.

They can be problem-solvers for applications where mineral oil products deteriorate too rapidly or lead to premature failures.

Texaco Pinnacle EP oils meet the requirements of:

  • U.S. Steel 224
  • AGMA 9005 and qualify as AGMA EP gear lubricants

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 222076; MSDS Number: 8611

Vendors:
Available Properties
  • API Gravity
  • Viscosity Measurement, Viscosity Index
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Timken Test, OK Load
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Pour Point
  • Flash Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
ChevronTexaco Corp

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.