MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Eastman Dymerex™ Polymerized Rosin
Categories: Polymer

Material Notes: Dymerex™ modified rosin is a pale, acidic, thermoplastic, high softening point resin. It is composed predominately of dimeric acids derived from rosin with lesser amounts of monomeric resin acids and neutral materials of rosin origin. Dymerex™ modified resin has high resistance to oxidation and does not crystallize from solutions or from solid compositions. It is compatible with many natural and synthetic film formers and rubbers. Being an acidic resin, it reacts readily with polyalcohols or hydrated lime to yield high melting derivatives.

Application/Uses:

  • Assembly
  • Bookbinding
  • Caulks and Sealants
  • Contact Adhesives
  • Footwear and Leather
  • Hot Melt Adhesives
  • Laminating
  • Pressure sensitive adhesives
  • Solventborne Adhesives
  • Tapes and Labels
  • Wire and Cable
Key Attributes:
  • Alcohol-soluble
  • Non-crystalline
  • Resistant to oxidation
  • Thermoplastic rosin acid
  • Very high softening point

Information provided by Eastman

Vendors:
Available Properties
  • Density
  • Brookfield Viscosity, Thermosel, Melt
  • Brookfield Viscosity, Thermosel, Melt
  • Brookfield Viscosity, Thermosel, Melt
  • Brookfield Viscosity, Thermosel, Melt
  • Molecular Weight, Mn
  • Molecular Weight, Mw; Mw/Mn = 1.18
  • Molecular Weight, Mz
  • Total Acid Number, [mg KOH/g]
  • Ring & Ball Softening Point, ASTM E 28
  • Gardner Color Number, 50% resins solids in toluene or xylene
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Eastman Chemical Company

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.