MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Vinnolit® E 70 TT PVC for Paste Making
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Vinnolit® E 70 TT PVC for paste making resin. Vinnolit® E 70 TT is a fine particle homopolymeric emulsion grade, designed for paste applications. It can be easily converted into a plastisol with very low viscosity (over broad shear range), strictly Newtonian flow behavior and excellent shelf life, with medium plasticizer contents it exhibits no yield point or flow anomalies. Due to its general flow characteristics, the low paste viscosity level, the very neutral color appearance and the excellent low water absorption, Vinnolit® E 70 TT is perfectly useful for textile coatings (waterproofs, sun sails, tarpaulins, conveyor belts etc.), artificial leather and flooring top coats as well as for rotational molding and dip coating processes. The product additionally shows an excellent contact transparency even in thick film applications. A very easy plastisol handling is completing the product profile. Remarkable properties of Vinnolit® E 70 TT are: very low viscosity over whole shear-area, Newtonian flow type, excellent low water absorption, very good contact transparency, low yellowing- or pinking effects with heat treatments over several weeks, neutral own-color, good miscibility with extender- or blending resins, good thermic stability, high stability of plastisol viscosity, easy plastisol handling.

Information provided by Vinnolit.

Vendors:
Available Properties
  • Volatiles, ISO 1269
  • Apparent Bulk Density, ISO 60
  • Particle Size, DIN EN ISO 53195, <= 2.0% Retained on 0.063 mm Sieve
  • Viscosity Test, ISO 1628-2, Reduced Viscosity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.