| NanoActive Al2O3 Plus is produced using proprietary processes to obtain high specific surface area, high porosity (75% are mesopores), low density, weakly aggregated material possessing high adsorption capacity and chemical reactivity. Applications: Applications include air cleaning, catalysts supports, coatings and binders, destruction of chemical warfare agents, heat transfer fluids (suspensions), polishing materials, polymer nanocomposites for improved tribological performance, smoke obscurant, and structural ceramics. Information provided by NanoScale Composition based on metal |