| Hostacom 515-UV BLK high melt flow, 2,100 MPa flexural modulus, UV-stabilized, 15% talc-filled polypropylene copolymer has a balance of properties. It is typically used for automotive interior trim applications. This material processes very well and provides parts with outstanding surface appearance. Availability: North America Application: Automotive Parts; Interior Automotive Applications Market: Automotive Processing Method: Injection Molding Attribute: Copolymer; Good Dimensional Stability; Good Moldability; Good Weather Resistance; High Flow; High Rigidity; Pleasing Surface Appearance Information provided by LyondellBasell. |