| Lupolen 2221F is a fractional melt index homopolymer LDPE resin designed for film applications requiring an excellent balance of clarity, stiffness, shrink and strength. 2221F is selected by customers for collation shrink films, pallet shrink films, packaging films and heavy duty films where clarity and stiffness are important. 2221F contains an antioxidant. Availability: Africa-Middle East; Asia-Pacific Application: Bags & Pouches; Clarity Film; Film Wrap; Food Packaging Film; Heavy Duty Packaging; Industrial Film; Lamination Film; Shrink Film; Surface Protection Film Market: Flexible Packaging Processing Method: Blown Film Information provided by LyondellBasell. |