MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
General Plastics LAST-A-FOAM® TF-6070-8.5 Polyurethane Foam
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: TF6070 High-density Series: These foams are designed for shock isolation of heavy objects when the supporting foam will be under Long term static stress. The TF6070 Series offers excellent shock isolation with minimum creep while under continuous static stress loads that range from 0.2 to 10.0 psi. Like other LASTAFOAM ® TF-series High-density polyether polyurethane foams, the TF6070 Series is formulated to absorb large amounts of energy while protecting payloads from high stress levels. It is quite firm in relation to its density and features relatively flat static-and dynamic-stress-versus-deflection curves. Except under conditions of intense UV radiation, these polyetherurethane formulations are highly durable and resistant to environmental factors, maintaining consistent performance. Elevated temperatures have no long-term effects up to 180°F, but these foams do lose approximately 10% in firmness at the higher temperature. Reduced temperatures also have negligible effects except at subzero temperatures, when the foam can become significantly firmer.
Shock Isolation Polyurethane Foam Applications: LASTAFOAM ® TF6070 products serve applications that do not require flame-retardant foam. General Plastics has supplied large quantities of these flexible foam products for use in the Minuteman program as shock isolation of the missile and instrument floor. They have also been used widely as dunnage for nuclear warhead shipping and storage containers. For a flame-resistant version with similar properties, opt for LASTAFOAM ® TF5070 products. Their performance parallels TF6070 open-cell polyurethane foams, except for the need to use a slightly higher foam density under equal conditions. These products are available as sheets, blocks and molded parts.

Advantages:

  • Supports heavy objects under ongoing static stress
  • Absorbs large amounts of energy
  • Offers excellent shock isolation
  • Exhibits minimal foam creep
  • Long-lasting Performance
  • Largely unaffected in applications up to 180 ºF
  • Missile shock isolation
  • Missile instrument floor shock isolation
  • Nuclear warhead shipping pad
  • Nuclear warhead storage pads

Information provided by General Plastics Manufacturing Company

Vendors:
Available Properties
  • Density
  • Maximum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.