| Fair to excellent corrosion resistance. Good hot workability for hot forging, pressing, and machining operations. Applications: marine hardware, screw machine products, valve stems. Test specimen: bar - 38mm diameter. |
| ISO CuZn37Pb1Sn1, ISO CuZn36Sn1Pb, CEN CW712R, CEN CW714R |