MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Fibre Glast 2000 / 2020 System 2000 Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, Molded, Glass Fiber Filler

Material Notes: System 2000 Epoxy Resin is a low viscosity, light amber laminating resin that is designed for fabricating parts and other demanding structural applications. Use this system to maximize the physical properties of carbon fiber, Kevlar®, and glass laminates! Test results have proven superiority over other room temperature epoxies. Its low viscosity and great handling characteristics make it a favorite in the shop too!

Three high performance hardener systems are available for the System 2000 resin. 20 minute, 60 minute, and 120 minute pot life versions are all options. This added variety allows the fabricator to select the system best suited to the size, complexity or time-frame of the project. Simple parts which need to be demolded quickly should use the 20 minute hardener. Larger and more complex parts can use either of the other hardeners.

Vacuum bagging applications would typically warrant the longest 2 hour working time. As with any epoxy system, adhere to the proper mix ratios and maintain an adequate curing temperature of at least 70°F. The cure time will be cut in half for every 10°F that the temperature is raised above 70°F.

The short 20 minute pot life of the 2020 Epoxy Hardener is quite versatile. Use for repairs, simple fabrications, or those parts requiring a quick demold time.

Information provided by Fibre Glast Developments Corporation.

Vendors:
Available Properties
  • Density
  • Viscosity, ASTM D2293
  • Hardness, Shore D, ASTM D2240, Cured
  • Tensile Strength at Break, ASTM D638, Property derived with 10 Ply Laminate, hand Lay-up, Style 181 Glass Fabric, 55% Glass Content.
  • Elongation at Break, ASTM D638, Property derived with 10 Ply Laminate, hand Lay-up, Style 181 Glass Fabric, 55% Glass Content.
  • Tensile Modulus, Property derived with 10 Ply Laminate, hand Lay-up, Style 181 Glass Fabric, 55% Glass Content.
  • Flexural Strength, ASTM D790, Property derived with 10 Ply Laminate, hand Lay-up, Style 181 Glass Fabric, 55% Glass Content.
  • Flexural Modulus, ASTM D790, Property derived with 10 Ply Laminate, hand Lay-up, Style 181 Glass Fabric, 55% Glass Content.
  • CTE, linear, ASTM D696
  • Glass Transition Temp, Tg
  • Pot Life, ASTM D2471, 4 fl. Oz.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Fibre Glast Developments Corporation

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.