MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
Lanxess Uniplex DBS Plastic Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Uniplex DBS is an efficient, low-temperature-resistant plasticizer for a variety of polymers, namely cellulose esters, polyvinyl butyral, polyvinyl chloride, polyvinylidene chloride, polystyrene, and rubber.

Chemical composition: Di-butyl Sebacate

CAS reg. no.: 109-43-3

General Uniplex DBS has excellent compatibility with a range of polymers with superior properties at low temperatures. It has a low viscosity, enabling the manufacture of highly filled pigment batches. Uniplex DBS is an excellent choice as a replacement for Dibutyl Phthalate in a number of applications, inclusive PVC where it offers a good gelling capacity. Uniplex DBS is used when regulations and recommendations governing food contacting applications need to be met.

Applications: Uniplex DBS is a general purpose plasticizer for variety of plastics, namely cellulose esters (cellulose acetate butyrate, cellulose acetate propionate, ethyl cellulose), polyvinyl butyral, polyvinyl chloride, polyvinylidene chloride, polystyrene, and synthetic rubbers (especially nitrile and chloroprene). It can be used as a dispersant for pigments in various plastics.

Information provided by Lanxess.

Vendors:
Available Properties
  • Density
  • Viscosity
  • Melting Point
  • Refractive Index
  • Moisture Content, Karl Fischer
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Lanxess, Spinoff of Bayer

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.