| Capran® 1500 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbons, and many solvents. It is also microwavable, making it an excellent choice for lidding stock. Applications: bag-on-box packaging, packaging for processed meats, cheese, meat snacks, coffee bricks, coffee bags, and pet food, agricultural bags, stand-up shampoo pouches, book covers and metallized balloons. Former Honeywell product; AdvanSix is a spin-off of Honeywell. |