MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Phillips 66 Kendall® L-427 Super Blu® NLGI Grade 2
Categories: Fluid; Lubricant; Lithium Gellant

Material Notes: Kendall® L-427 Super Blu is a high-quality, multipurpose, extreme-pressure (EP) lithium complex grease developed for the lubrication of automotive and industrial equipment operating under heavy loads and at moderate to high temperatures. It is NLGI GC-LB certified for use as a multipurpose automotive wheel bearing and chassis lubricant. L-427 Super Blu is manufactured with high-quality paraffinic base oils thickened with lithium complex soap. It is fortified with extreme-pressure and antiwear additives, a tackifier, and rust and oxidation inhibitors to provide excellent wear protection, excellent thermal stability at high temperatures, and excellent resistance to corrosion and water washout. It forms an effective seal to help minimize bearing contamination and provides a high level of adhesion to the bearing surface for improved retention, reduced leakage and enhanced resistance to water washout.

Applications:

  • Wheel bearings of passenger cars, trucks, high-performance vehicles, sport utility vehicles and motorcycles, particularly vehicles with disc brakes
  • Ball joints, universal joints, other chassis parts and water pumps on passenger cars, trucks and other mobile equipment
  • Heavily loaded plain and rolling-element bearings in industrial and mobile equipment
Features/Benefits:
  • Excellent performance over a wide temperature range
  • High load-carrying capacity
  • Excellent wear protection
  • Protects against rust and corrosion
  • Excellent resistance to water washout
  • NLGI GC-LB certified

Information provided by Phillips 66 Lubricants.

Vendors:
Available Properties
  • Density
  • Viscosity Measurement, Index
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Oxidative Stability, ASTM D942, Pressure Drop
  • Four Ball Extreme Pressure, Weld Load, ASTM D2596
  • Four Ball Wear, ASTM D4172, Scar Diameter
  • Penetration P(60), 1/10 mm, ASTM D217
  • Timken Test, ASTM D2782
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Dropping Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.