Temper: Nominal Grain Size 0.035 mm Fabrication Properties: Excellent Suitability – Soldering; Good Suitability – Brazing,, Capacity for Being Cold Worked, Capacity for Being Hot Formed; Fair Suitability – Oxyacetylene Welding, Gas Shielded Arc Welding, Butt Weld Common Fabrication Processes: Cold - Drawing, machining, moderate cold heading; Hot - Extrusion, forging (closed die only) Typical uses: Fire Protection; Electrical Connectors; Motor Parts; Soldering Copper; Switch Parts; Transistor Bases; Forgings; Furnace Brazed Articles; Soldering Tips; Welding Torch Tips; Fixtures; Plumbing Fittings; Sprinkler Heads Applicable Specifications: ASTM B224; Bar – Forgings ASTM B124/B124M, ASTM B301/B301M; Brazing Filler Metal – FEDERAL QQ-B-650; Die – Forgings ASTM B283/B283M; Fitting – ASME B16.22; Forgings, Die (Hot Pressed) – ASME SB283; Rod – ASTM B301/B301M, SAE J463, Forgings ASTM B124/B124M, SAE J461; Shapes – ASTM B301/B301M, ASTM B216, Forgings ASTM B124/B124M; Wire – ASTM B301/B301M |