MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Foster ProPell™ Low Friction ProFlex™ 35A SEBS
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: ProFlex™ is a comprehensive range of Styrene Ethylene Butylene Styrene (SEBS) Thermoplastic Elastomers (TPEs). These unique polymers offer excellent elastomeric properties, with design flexibility and ease of processing via injection molding and extrusion. ProFlex™ SEBS is available in standard, tear resistant, and ProPell™ formulations across a range of durometers. Foster can also customize formulations if the application requires it. ProFlex™ SEBS was designed to be used in a variety of medical applications including catheters, surgical handles and ergonomic grips. ProFlex™ SEBS is available in a variety of development quantities upon request.

Information provided by Foster Corporation

Vendors:
Available Properties
  • Hardness, Shore A, ASTM D2240
  • Tensile Strength at Break, ASTM D412
  • Tensile Strength, ASTM D412
  • Elongation at Break, ASTM D412
  • Tensile Modulus, ASTM D638
  • Coefficient of Friction, ASTM D1894, Stainless Steel
  • Tear Strength, ASTM D624
  • Rear Barrel Temperature, Injection
  • Rear Barrel Temperature, Extrusion
  • Middle Barrel Temperature, Injection
  • Middle Barrel Temperature, Extrusion
  • Front Barrel Temperature, Injection
  • Front Barrel Temperature, Extrusion
  • Nozzle Temperature, Injection
  • Die Temperature, Extrusion
  • Mold Temperature, Injection
  • Screw Speed, Injection
  • Screw Speed, Extrusion
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
Thermoplastic Elastomer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.