MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Phillips 66 Multipurpose R&O Oil ISO Grade 32
Categories: Fluid; Lubricant

Material Notes: Multipurpose R&O Oil is a rust and oxidation (R&O)-inhibited, antiwear circulating oil developed for use in circulation systems, centrifugal air compressors, geared turbines, lightly loaded enclosed gear drives and many other industrial applications. It contains a low level of ashless (zinc-free) antiwear additive for mild wear protection. Multipurpose R&O Oil is formulated to provide protection against rust, corrosion and deposit formation, plus mild wear protection. It has good oxidation resistance at high temperatures to minimize sludge and varnish formation, resulting in long service life. It protects system components against rust and corrosion. It has excellent water-separating properties to minimize the formation of emulsions, and is resistant to excessive foam buildup that can interfere with proper lubrication. An ashless antiwear additive provides mild wear protection to help increase equipment life.

Applications:

  • Air tools and other pneumatic equipment lubricated through air line lubricators
  • Centrifugal air compressors
  • Steam turbines and hydroelectric turbines, both direct-drive and with gear drives
  • Lightly loaded enclosed industrial gearboxes where the OEM specifies a R&O type oil (ISO VG 68 and higher, typically)
  • Lightly loaded plain and rolling-element bearings, such as those in electric motors and blowers
  • Vacuum pumps, deep-well water pumps and machine tools
  • General-purpose machinery and shop lubrication
Multipurpose R&O Oil meets the requirements of the following industry and OEM specifications:
  • ABB G12106
  • AGMA Grades 0 through 7 (non-EP)
  • Alstom Power HTGD 90 117 for geared turbines
  • ASTM D4304 Type I Turbine Oil (ISO VG 32, 46, 68, 100)
  • British Standard 489
  • Denison Hydraulics HF-1
  • DIN 51517 Part 1, Lubricating Oils, Type CL
  • DIN 51524 Part 1, Hydraulic Oils, Type HL
  • General Electric GEK 101941A, GEK 46506e, GEK 27070 (obsolete), GEK 28143A (obsolete)
  • Ingersoll-Rand Centak centrifugal compressors
  • Solar Turbines ES 9-224 Class II Turbine Oil
  • U.S. Military MIL-L-17672D
  • U.S. Steel 126
Features/Benefit:
  • Good oxidation resistance to minimize sludge and varnish formation
  • Mild wear protection
  • Protects against rust and corrosion
  • Excellent water-separating properties
  • Low carbon-forming tendency for use in centrifugal air compressors
  • Good foam resistance

Information provided by Phillips 66 Lubricants.

Vendors:
Available Properties
  • Specific Gravity
  • Density
  • Viscosity Measurement, Index
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Oxidative Stability, ASTM D2272, RPVOT
  • Oxidative Stability, ASTM D943-04a, TOST
  • ASTM Color, ASTM D1500
  • Total Acid Number, ASTM D974, [mg KOH/g]
  • Four Ball Wear, ASTM D2266, Scar Diameter
  • Pour Point
  • Flash Point, COC
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.