Applications: Injection moulded housings, boxes and technical parts. PRE-ELEC® PA 1408 is well suited for applications where the good mechanical properties of polyamide are required.
Processing: PRE-ELEC® PA 1408 compound can be processed in the injection moulding machines using normal processing conditions as with polyamide.Test Specimen: 10[mm] wide moulded rod
This page displays only the textof a material data sheet.To see MatWeb's complete datasheet for this material (includingmaterial property data, metalcompositions, material suppliers,etc), please click the button below.
Category NotesPlasticPA, Polyamide