| Description Polyfort® FPP 1068-32 Black is a 40% mineral filled polypropylene designed for use when improved heat resistance, dimensional stability and high stiffness is needed. Application Applications of FPP 1068-32 include electrical connections, ducts, impeller and housings. Information provided by A. Schulman. LyondellBasell has acquired A. Schulman, Inc.. |