MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
KLJ Group KLJ-XL-33 XLPE
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: KLJ-XL compounds are a combination of LLDPE base material and catalyst master batch. The base polymer LLDPE is grafted with Vinyl Silane. The process results in moisture/ambient curable polymer having excellent processing characteristics without any volatiles. When properly mixed, addition of 5 parts of corresponding catalyst materbatch to 95 parts of grafted polymer, an insulation with excellent thermo-oxidative stability is achieved.

Application: Grafted polymer & corresponding catalyst masterbatch of each grade is designed for insulation of low voltage (up to 6 KVA)/medium voltage (up to 33 KVA) application and power cables.

Specifications: Grafted polymer in combination with corresponding catalyst masterbatch meets the following specifications, when processed using sound extrusion practice and testing procedures.

IEC-60502, IS-7098 (Part-I & II), IS 3396

Information provided by KLJ Group

Vendors:
Available Properties
  • Deformation, IS 10810 Part 30/IEC 60502
  • Tensile Strength, IS 10810 Part 7/IEC 60502
  • Tensile Strength, IS 10810 Part 11/IEC 60502
  • Elongation at Break, IS 10810 Part 30/IEC 60502, Under Load
  • Elongation at Break, IS 10810 Part 7/IEC 60502
  • Elongation at Break, IS 10810 Part 11, Cold Elongation Test
  • Elongation at Break, IS 10810 Part 11/IEC 60502
  • Volume Resistivity, IS 3396
  • Dielectric Constant, IEC 60250
  • Dielectric Strength, IEC 60243
  • Dissipation Factor, IEC 60250
  • Shrinkage, IS 10810 Part 30/IEC 60502
  • Zone 1
  • Zone 2
  • Zone 3
  • Zone 4
  • Zone 5
  • Die Temperature
  • Head Temperature
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.