MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
ChevronTexaco PRO-GARD® Fuel Injector Cleaner
Categories: Fluid; Lubricant

Material Notes: Features

Engines that are sensitive or in severe service can have performance problems caused by fuel injector deposits. Improvements in gasoline that became mandatory January 1, 1995, may not solve all of these problems. Chevron PRO-GARD Fuel Injector Cleaner with its exclusive Chevron TECHRON® technology can remove deposits form clogged fuel injectors in one tankful. Fuel injector deposits at the injector tip can impact fuel flow, upsetting the air/fuel mixture. The symptoms of these deposits can be:

  • Hesitation or stumble during acceleration
  • Loss of power
  • Increased emissions of hydrocarbons and carbon monoxide
Chevron PRO-GARD Fuel Injector Cleaner can clean up these deposits in one tankful.

Applications

Chevron PRO-GARD Fuel Injector Cleaner is designed for all carbureted or fuel injected spark ignition engines.

Safe to use every 1,000 miles or as needed to keep fuel injectors clean

Not recommended for air-cooled two-stroke engines.

TECHRON and PRO-GARD are registered trademarks of Chevron Corporation.

Vendors:
Available Properties
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
ChevronTexaco Corp

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.