MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Ti-25Al-10Nb-3V-1Mo Titanium Aluminide
Categories: Metal; Intermetallic; Nonferrous Metal; Titanium Alloy

Material Notes: Alpha-2 Titanium Aluminide Ti3Al based alloy. Ti-25Al-10Nb-3V-1Mo refers to the atomic percentage composition. The niobium addition improves stress rupture and elevated temperature strength versus Ti3Al, while the molybdenum addition also increases the elevated temperature strength. Intermetallic aluminides have good mechanical properties and stability to be used in high temperature environments. A thin protective Al2O3 coating forms to provide oxidative stability.

Vendors:
Available Properties
  • Tensile Strength, Ultimate, Colony structure, primary alpha-2 grains
  • Tensile Strength, Ultimate, Fine Widmanstätten microstructure
  • Tensile Strength, Ultimate, Widmanstätten microstructure, primary alpha-2 grains
  • Tensile Strength, Ultimate, Widmanstätten microstructure
  • Tensile Strength, Ultimate, Fine Widmanstätten microstructure, primary alpha-2 grains
  • Tensile Strength, Yield, Colony structure, primary alpha-2 grains
  • Tensile Strength, Yield, Widmanstätten microstructure, primary alpha-2 grains
  • Tensile Strength, Yield, Fine Widmanstätten microstructure
  • Tensile Strength, Yield, Widmanstätten microstructure
  • Tensile Strength, Yield, Fine Widmanstätten microstructure, primary alpha-2 grains
  • Elongation at Break, Fine Widmanstätten microstructure
  • Elongation at Break, Colony structure, primary alpha-2 grains
  • Elongation at Break, Widmanstätten microstructure
  • Elongation at Break, Widmanstätten microstructure, primary alpha-2 grains
  • Elongation at Break, Fine Widmanstätten microstructure, primary alpha-2 grains
  • Creep Strength, Creep Rupture, Widmanstätten microstructure
  • Fracture Toughness, KIC; Widmanstätten microstructure
  • Aluminum, Al, by weight
  • Molybdenum, Mo, by weight
  • Niobium, Nb (Columbium, Cb), by weight
  • Titanium, Ti, by weight
  • Vanadium, V, by weight
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Ensinger PEI
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.