| Clyrell EC5080 is a thermoplastic polyolefin, which has been developed for EBM and sheet/ thermoforming application. Clyrell EC5080 can overcome the limitations of conventional PP because of good low temp impact resistance with good transparency. Therefore, customer can contribute a differentiated competitiveness for extrusion blow molding/ sheet/ TF markets Product Features: Good low temperature impact resistance/ Good optical property Typical Applications: Blow Molding applications/ Sheet and Thermoforming applications Information provided by PolyMirae |