MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
LyondellBasell Sequel® E3400 SP Polyolefin
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Product Description: Sequel E3400 SP fractional melt flow, high flexural modulus, improved scratch resistance thermoplastic polyolefin (TPO) is designed for thermoformed exterior or interior applications that require low-temperature toughness and dimensional stability. This extrusion-grade material exhibits enhanced melt strength for a wide thermoforming processing window.

Availability: North America

Features: Good Dimensional Stability; Good Melt Strength; Good Scratch Resistance; Low Flow; Low Temperature Impact Resistance

Uses: Automotive Bumper; Automotive Exterior Parts; Automotive Interior Parts; Industrial Applications; Profiles

Processing Method: Extrusion; Thermoforming

Information provided by LyondellBasell Industries

Vendors:
Available Properties
  • Density, ISO 1183
  • Melt Flow, ISO 1133
  • Tensile Strength, Yield, ISO 527-2/50, 150x10x4 mm
  • Flexural Modulus, ISO 178, 80x10x4 mm
  • CTE, linear, Parallel to Flow, ASTM E228
  • CTE, linear, Transverse to Flow, ASTM E228
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
LyondellBasell LYB (former Equistar)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.