| KEBALLOY ECO XB 220404 R-PET is a recycled, medium viscosity PET grade (polyethylene terephthalate) approved for direct food applications. The material is supplied as crystallized granules. This grade is produced from 100% post-consumer bottle flakes and has a light green color. Properties: amorphous, dimensionally stable, compliant for food contact (according to 10/2011 EC), semi-crystalline, approved for food contact (EU and FDA) Typical areas of application: Glasses frames, Cover, Filter cups, Housing, Crockery and cutlery, industrial goods, Cosmetic packaging, Food packaging, Toys, Sports & Leisure Articles Industries: Household appliances, Industry, Agriculture, Food processing industry, Sanitary industry, Sports & Recreation Information provided by BARLOG plastics GmbH. |