| Flame-retardant bedding compound for XLPE insulation and HFFR sheathing Compound class: Bedding compound Based on: TPE-O Characteristics: Halogen free flame retardant Application examples: Insulation 2 XI 1; XLPE; acc. DIN / VDE 0207 part 22 2 YI 1 – 5; PE; acc. DIN / VDE 0207 part 2 9 YI 1; PP; acc. DIN / VDE 0207 part 7 Application examples: Sheathing 2 YM 3; HDPE; acc. DIN / VDE 0207 part 3 Typical applications: Bedding compound for cables and wire with max. 90°C operating temperature at conductor Features: For tandem process; Flame retardant; Halogen-free Information provided by Melos |