MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
TIMET TIMETAL® 230 Titanium Alloy (Ti-2.5Cu); Annealed
Categories: Metal; Nonferrous Metal; Titanium Alloy; Alpha/Near Alpha Titanium Alloy

Material Notes: Cold Formable Medium-Strength Alloy

Industry Specifications: Germany Aerospace: 3.7124. France: T-U2. UK Aerospace Specifications BA TA. 21, 22, 23.

Features: This binary, age hardening alloy combines the easy formability and weldability of commercially pure titanium with improved mechanical properties, particularly at temperatures up to 350°C. It is used in the annealed condition as sheet, forgings, and extrusions for fabricating components such as bypass ducts of gas-turbine engines. Its used spread to the airframe industry, following the development of an ageing treatment which raises room-temperature tensile properties by about 25%, and nearly doubles the elevated temperature properties. Such a material is particularly attractive since it can be formed in the soft condition, thus lowering fabrication costs. It is nonmagnetic.

Typical heat treatment for this alloy: Anneal at 790°C for 1 hour and air cool. Solution heat treatment at 805°C for 1 hour with a rapid air cool. Aging heat treatment at 400°C for 8-24 hours with an air cool and then for 8 hours at 475°C with air cool.

Data provided by TIMET.

Vendors:
Available Properties
  • Density, Typical
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Reduction of Area
  • Creep Strength
  • Creep Strength, 0.1% total plastic strain
  • Creep Strength, 0.1% total plastic strain
  • Creep Strength, 0.1% total plastic strain
  • Modulus of Elasticity, Typical
  • Fatigue Strength, Rod, smooth, direct stress
  • Fatigue Strength, Rod, rotating bend
  • Fatigue Strength, Sheet; Reverse Bend; (UTS = 864 MPa)
  • Bend Radius, Minimum, sheet
  • Electrical Resistivity
  • CTE, linear
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Beta Transus
  • Carbon, C
  • Copper, Cu
  • Hydrogen, H
  • Iron, Fe
  • Nitrogen, N
  • Other, each
  • Other, total
  • Oxygen, O
  • Titanium, Ti, Calculated as remainder
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.