MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Mallard Creek Polymers Tykote® 1019 Styrene-Butadiene Emulsion
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: Tykote® 1019 is a carboxylated styrene-butadiene emulsion that has a firm hand with excellent film strength properties. It is intended for use as a base polymer in the formulation of barrier coatings for paper and paperboard packaging. Tykote® 1019 imparts excellent water resistance, and has good adhesion to a wide variety of surfaces. Tykote® 1019 is recommended for use in paper and paperboard coatings where a high degree of water and water vapor resistance is needed. It may also be formulated into barrier laminating adhesives for paper-to-paper, paper-to-film, and foil-to-paper.

Regulartory Status: FDA components in food contact applications.

  • 175.105 indirect food additives
  • 176.170 components of paper and paperboard in contact with aqueous and fatty foods
  • 176.180 components of paper and paperboard in contact with dry food
Storage and Handling: Protect from freezing. Ideal storage temperature is 22°C (72°F). Read the Tykote® 1019 Material Safety Data Sheet before handling, storing, or using this product.

Information provided by Mallard Creek Polymers

Vendors:
Available Properties
  • Solids Content
  • Particle Size
  • pH
  • Brookfield Viscosity, #20/200
  • Glass Transition Temp, Tg
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.