| Description: Primer for digital printing Usage: DigiPrime® 6029 is a flexo and gravure ready coating used to optimize substrates for HP Indigo printing. This product provides excellent adhesion of HP Indigo Electroinks® to textured paper wine label substrates and label stock especially for those using the WS6000 series presses. Application data: DigiPrime® 6029 can be applied via flexo or gravure. For best results with heavily textured wine label substrates, a flexo application is preferred. The use of corona treatment prior to application is recommended. Food Contact Information when manufactured in the USA: FDA: 175.105: Components of adhesives 176.170: Components of paper and paperboard in contact with aqueous and fatty foods.(Restricted) 176.180: Components of paper and paperboard in contact with dry foods. When manufactured in Belgium product meets food contact regulations for: Europe: Euro. Res. AP(2004)1(Restricted) Food Contact Information when manufactured in Belgium: FDA: 175.105: Components of adhesives 176.170: Components of paper and paperboard in contact with aqueous and fatty foods. 176.180: Components of paper and paperboard in contact with dry foods. Information provided by Michelman® |