MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Syensqo (Solvay Specialty Polymers) Polidiemme® G/430 Polyolefin
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Polidiemme® XLPO-Cross-linkable Polyolefin elastomer based compound crosslinkable by ambient moisture, consisting of a silane pregrafted base compound to be used with a catalyst masterbatch (Sioplas® method). Standard complying: Cenelec HD 22.1 EI4, EI6, EI7 and EM3; Cenelec HD 603 DIH1; IEC 60502 EPR; IEC 60092/351 EPR; BS 7655 GP4, GP5 AND GP7, VDE 207/20 3GI3

Availability:

  • Asia Pacific
  • Europe
  • North America
Features:
  • Crosslinkable
  • Good Flexibility
Uses:
  • Cable Jacketing
  • Low Voltage Insulation
  • Wire & Cable Applications

Information provided by Solvay

Vendors:
Available Properties
  • Density, ASTM D792
  • Melt Flow
  • Hardness, Shore D, ISO 868
  • Tensile Strength at Break, IEC 60811
  • Tensile Strength at Break, IEC 60811, After Aging in Air Oven
  • Tensile Strength at Break, IEC 60811, After Aging in Air Oven
  • Tensile Strength at Break, IEC 60811, After Aging in Air Bomb, 0.55 MPa
  • Elongation at Break, IEC 60811
  • Elongation at Break, IEC 60811, After Aging in Air Oven
  • Elongation at Break, IEC 60811, After Aging in Air Oven
  • Elongation at Break, IEC 60811, After Aging in Air Bomb, 0.55 MPa
  • Volume Resistivity, IEC 60502
  • Volume Resistivity, IEC 60502
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149
  • Dissipation Factor, ASTM D150
  • Zone 1
  • Zone 2
  • Zone 3
  • Zone 4
  • Die Temperature
  • Head Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay Specialty Polymers (includes former Solexis)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.