MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Akrochem Sterling® Blacks NS Carbon Black
Categories: Carbon; Carbon Black

Material Notes: Product Description: This line of Sterling carbon blacks manufactured by Cabot Corporation are the cleanest version of standard grade carbon blacks. Sterling grade carbon blacks are classified as semi-reinforcing with the exception of Sterling C which is a conductive black. During careful manufacturing techniques, the impurities of the standard grade blacks are reduced. Impurities like hard particle carbon grit, metallic rust, stainless steel, aluminum salts, sulfur, etc. do affect physical and surface properties of elastomeric vulcanizates. Compounders have seen physical improvements especially in dynamic properties (flex fatigue), ECD (electrochemical degradation), tensile strength, elongation, tan delta, surface appearance, hot tear resistance, etc. utilizing these carbon blacks. Also, due to their cleaner nature, these blacks have contributed to smoother injection, extruded and compression molded stocks, lower scrap rates, improved dispersion, fewer screen changes and less wear on production equipment. Compounders choose carbon blacks basically by Iodine and DBP values. Iodine number represents the black’s surface area. The higher the number, the more surface area is available to reinforce the rubber matrix. This affects failure properties like abrasion, tear, tensile strength, etc. The DBP number represents the structure (bulkiness) of the black. Again, the higher DBP number equates to higher structure. This affects non-failure properties like modulus, die swell, loading capacity, conductivity and especially dispersion. The chart below lists typical values and applications for various standard ASTM grade carbon blacks cross-referenced with Sterling products available from Akrochem.

Application: Gaskets, seals, wiper blades, hose, extruded profiles

Information provided by Akrochem Corporation

Vendors:
Available Properties
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.