MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Solvay FM® 350NA Adhesive Foam
Categories: Polymer; Adhesive

Material Notes: Description: FM® 350NA adhesive film is an aluminum-filled structural adhesive designed for elevated service temperatures. It was developed specifically for engine nacelle applications demanding continuous mechanical performance at 350°F (177°C). The FM 350NA adhesive product group optimizes bonding capabilities of metal honeycomb sandwich structures, especially those involving a perforated metal skin. Cytec’s BR®154 and BR® 6750 corrosion inhibiting primers are recommended for use with FM 350NA adhesive films in bonding aluminum details. FM 350NA is supplied on a light-weight glass carrier (FM 350NA) or as an unsupported film (FM 350NAU). Both forms provide superior flow properties without the use of asbestos as a thixatrope. FM 350NA adhesive, when properly cured at 340°F – 365°F (171°C – 185°C), exhibits impressive service properties, as exemplified by the test results reported in the attached tabulations.

Features & Benefits:

  • Structural properties from -67°F to 350°F (-55°C to 177°C)
  • Superior resistance to long-term thermal environment exposure
  • Unsupported film reticulates easily when heated
Applications:
  • Engine nacelle bonding
  • Acoustic applications

Information provided by Cytec, subsequently acquired by Solvay.

Vendors:
Available Properties
  • Volatiles
  • Storage Temperature
  • Tensile Strength, Flatwise, After exposure to 3,000 hours at 350°F (177°C)
  • Tensile Strength, Flatwise, After exposure to 3,000 hours at 350°F (177°C)
  • Tensile Strength, Flatwise
  • Tensile Strength, Flatwise
  • Tensile Strength, Flatwise
  • Shear Strength, Lap, Relative Humidity 98% Fluid 7 days at 158°F(70°C), 3/8 inch core
  • Shear Strength, Lap, Salt Spray, 5% 30 days at 95°F (35°C), 3/8 inch core
  • Shear Strength, Lap, Hydrocarbon Test (TT-S-735, Type II) Fluid 7 days at 158°F (79°C), 3/8 inch core
  • Shear Strength, Lap, MIL H-5606 Fluid 7 days at 77°F (25°C), 3/8 inch core
  • Shear Strength, Lap, JP-5 Jet Fluid 7 days at 77°F (25°C, 3/8 inch core
  • Shear Strength, Lap, Relative Humidity 98% Fluid 7 days at 158°F(70°C)
  • Shear Strength, Lap, Salt Spray, 5% 30 days at 95°F (35°C)
  • Shear Strength, Lap, JP-5 Jet Fluid 7 days at 77°F (25°C)
  • Shear Strength, Lap, Hydrocarbon Test (TT-S-735, Type II) Fluid 7 days at 158°F (79°C)
  • Shear Strength, Lap, MIL H-5606 Fluid 7 days at 77°F (25°C)
  • Shear Strength
  • Shear Strength, Lap, After exposure to 3,000 hours at 350°F (177°C)
  • Shear Strength, Lap, After exposure to 3,000 hours at 350°F (177°C)
  • Shear Strength
  • Shear Strength
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay, former Rhodia Engineering Plastics

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.