MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
3M Scotch-Weld™ DP807 Acrylic Adhesives
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: 3M™ Scotch-Weld™ Acrylic Adhesive DP807 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and bond well to many metals, ceramics, wood and most plastics with minimal surface preparation.

Information provided by 3M

Vendors:
Available Properties
  • Viscosity, Base
  • Viscosity, Accelerator
  • Hardness, Shore D
  • Shear Strength, Overlap, Etched Aluminum tested after 1 week of Immersion in Toluene
  • Shear Strength, Overlap, PC, Substrate Failure
  • Shear Strength, Overlap, ABS, Substrate Failure
  • Shear Strength, Overlap, Acrylic, Substrate Failure
  • Shear Strength, Overlap, PVC, Substrate Failure
  • Shear Strength, Overlap, Etched Aluminum tested after 1 week of Immersion in 66°C tap water
  • Shear Strength, Overlap, Cold-Rolled Steel - slightly oily, Cohesive Failure
  • Shear Strength, Overlap, Etched Aluminum tested after 1 week of Immersion in Unleaded gasoline
  • Shear Strength, Overlap, Green Fiberglass Reinforced Plastic, Adhesive Failure
  • Shear Strength, Overlap, Cold-Rolled Steel - solvent cleaned, Adhesive Failure
  • Shear Strength, Overlap, Etched Aluminum tested after 1 week of Immersion in 66°C and 80% RH
  • Shear Strength, Overlap, Stainless Steel, Adhesive Failure
  • Shear Strength, Overlap, Aluminum - abraded, 150 grit sandpaper, Adhesive Failure
  • Shear Strength, Overlap, Etched Aluminum tested after 1 week of Immersion in IPA
  • Shear Strength, Overlap, Etched Aluminum tested after 1 week of Immersion in 20% bleach solution
  • Shear Strength, Overlap, Aluminum - etched, Adhesive Failure
  • Shear Strength, Overlap, Aluminum - bare, Adhesive Failure
  • Shear Strength, Overlap, Etched Aluminum cured for 7 days @ RT
  • Shear Strength, Overlap, Etched Aluminum tested after 1 week of Immersion in Diesel fuel
  • Shear Strength, Overlap, Etched Aluminum tested after 1 week of Immersion in 50% Antifreeze
  • Shear Strength, Overlap, Etched Aluminum
  • Shear Strength, Overlap, Etched Aluminum
  • Shear Strength, Overlap, Etched Aluminum
  • Shear Strength, Overlap, Etched Aluminum
  • Peel Strength, Etched Al/Etched Al after 1 week at RT cure
  • Dielectric Strength, ASTM D149
  • Cure Time, Full cure
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.