MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Lord Adhesives CircuitSAF™ MA-420 Epoxy Surface Mount Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: CircuitSAF™ MA-420 is an epoxy surface mount adhesive that cures rapidly at elevated temperatures and has been designed for use in high speed printed circuit board assembly for the attachment of surface mount components. This product is unique in that it can be used for both high speed dispensing and rapid printing without sacrificing any performance in either application. The high shear thinning and excellent viscosity recovery makes the material an excellent choice for high speed SMT applications. CircuitSAF™ MA-420 has been successfully used in high speed placement systems with integrated dispense heads. A list of equipment and the corresponding packaging can be found in the CircuitSAF™ MA-420 Brochure. CircuitSAF™ MA-420 also shows superior performance in non-contact dispense systems such as the Asymtek Dispense JetTM. The superior dot profile and high dot aspect ratio make it ideal for rapid printing. CircuitSAF™ MA-420 is fully compatible with the DEK ProFlow DirEKt ImagingTM system and is available in DEK ProFlowTM Cassettes.

All information provided by Lord.

Vendors:
Available Properties
  • Density
  • Particle Size, mean particle size, 5 microns
  • Brookfield Viscosity, 2HB CP52 Spindle @ 4.6rpm
  • Brookfield Viscosity, 2HB CP52 Spindle @ 0.1rpm
  • Modulus of Elasticity, DMTA @ 1kHz
  • Shear Strength, IPC817, 5 min 125ºC cure
  • Volume Resistivity
  • Insulation Resistance, After 4 days
  • Insulation Resistance, After 7 days
  • Dielectric Constant, ASTM D150-95
  • Dielectric Constant, ASTM D2520-95
  • Dielectric Constant, ASTM D2520-95
  • Dielectric Constant, ASTM D2520-95
  • Dielectric Constant, ASTM D150-95
  • Dielectric Strength, ASTM D149-97a
  • Dissipation Factor, ASTM D2520-95
  • Dissipation Factor, ASTM D2520-95
  • Dissipation Factor, ASTM D150-95
  • Dissipation Factor, ASTM D150-95
  • Dissipation Factor, ASTM D2520-95
  • CTE, linear, Alpha 1
  • CTE, linear, Alpha 2
  • Thermal Conductivity
  • Glass Transition Temp, Tg
  • Flash Point
  • Cure Time
  • Cure Time
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.