MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Phillips 66 Transmission Oil 90
Categories: Fluid; Lubricant

Material Notes: Conoco® Transmission Oil 90 is an SAE 90 mineral oil gear lubricant recommended for use in manual transmissions, transfer cases and rear axle assemblies of automotive, farm and off-highway equipment where the manufacturer specifies an API GL-1 gear oil. It also may be used in light-duty industrial applications where a non-compounded, ISO VG 150 or AGMA 4 mineral oil is specified. Transmission Oil 90 has good film strength and rust inhibition to protect gears, bearings and synchronizers. It also has good oxidation resistance to help minimize deposit formation, and good resistance to foaming.

Applications:

  • Heavy-duty, multiple-speed manual transmissions and transfer cases in trucks and buses where the manufacturer specifies an API GL-1, SAE 90 gear oil
  • Lightly loaded enclosed industrial gear drives where the OEM specifies a R&O type, AGMA 4 gear oil
  • General-purpose lubrication in applications that require a non-compounded, ISO VG 150 mineral oil
Transmission Oil 90 meets the requirements of:
  • API Service GL-1
Features/Benefits:
  • Good film strength for wear protection
  • Good oxidation resistance
  • Protects against rust and corrosion
  • Good foam resistance

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012, and branding was further reorganized in 2016. The Conoco® trade name is no longer in use but products may be available under different names.

Vendors:
Available Properties
  • Specific Gravity
  • API Gravity
  • Viscosity Measurement, Viscosity Index
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • ASTM Color
  • ASTM Color, ASTM D1500
  • Pour Point
  • Flash Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.