MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
LyondellBasell Premi-Glas® 1286 Glass Reinforced SMC
Categories: Polymer; Thermoset; Composite SMC; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass SMC

Material Notes: Premi-Glas® 1286 is a glass reinforced thermoset sheet molding compound designed for automotive under the hood applications.

Key features and benefits:

  • Designed for compression molding for optimal strength on large-span covers
  • Excellent resistance to automotive chemicals and fluids, and to salt spray
  • Replaces cast metals for reduced Noise, Vibration and Harshness, plus molded-in color
  • Meets the requirements of GMP.UP.018
  • Excellent thermal properties and elevated temperature modulus retention
  • Based on proprietary resin matrix for peak thermal performance

Market: Composite PowerTrain

Information provided by Premix.

This LyondellBasell product line was formerly a product of Premix and of A. Schulman.

Vendors:
Available Properties
  • Specific Gravity
  • Specific Gravity
  • Water Absorption, ISO 62
  • Linear Mold Shrinkage, Polymerization Shrinkage
  • Linear Mold Shrinkage
  • Tensile Strength
  • Tensile Strength, ISO 527
  • Tensile Strength, ISO 527
  • Tensile Modulus
  • Tensile Modulus, ISO 527
  • Tensile Modulus, ISO 527
  • Flexural Strength
  • Flexural Strength, ISO 178
  • Flexural Strength, ISO 178
  • Flexural Modulus
  • Flexural Modulus, ISO 178
  • Flexural Modulus, ISO 178
  • Poissons Ratio
  • Shear Modulus, Calculated
  • Izod Impact, Unnotched, ASTM D4812
  • Izod Impact, Unnotched
  • Impact, ISO 6603-2, (kN) High Speed Impact (Impact at max load)
  • Impact, ISO 6603-2, (mm) High Speed Impact (Deflection at max load)
  • Instrumented Impact Total Energy, ISO 6603-2, High Speed Impact (Total energy)
  • Instrumented Impact Energy at Peak, ISO 6603-2, High Speed Impact (Energy at max load)
  • CTE, linear, Parallel to Flow, Z Direction
  • CTE, linear, Transverse to Flow, XY Direction
  • Thermal Conductivity
  • Glass Transition Temp, Tg, ISO 6721 DMS
  • Glass Transition Temp, Tg
  • Processing Temperature, Compression Molding
  • Clamp Pressure, Molding Pressure
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
LyondellBasell, former A. Schulman (Premix)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.