| MGB-A75E is a room-temperature-mixable, semi-high-performance polyether polyurethane system. The material is specifically designed so that the user can manually mix the component during the relatively long pot-life. The cured elastomer products exhibit high rebound and good stability in the outdoor environments. This combination of features makes MGB-A75E a good raw material candidate to make roller skate/inline skate wheels, cruse board/long board wheels, liners/bumpers used outdoors and in wet conditions as well as many specialty products. This formulation is designed to be used in smaller operations without dispensing equipment making a smaller quantity of products. For a larger production rate, please consider using MGG-A70DQ for a faster mold cycle and more enhanced physical properties. MGB-A75E Part-A (Isocyanate) Component: MGE-067 Part-B (Curative) Component: BAN-005POR16 Mixing Ratio: 1.00: 0.07 = Part-A: Part-B by volume 1.00: 0.069 by weight 7:100 Gear Ratio for Gear Information provided by Northstar Polymers |