MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
CRP  Windform
Mitsubishi PA-CX12 3D Printing Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: PA-CX12 is a high-performance nylon filament with a broad range of mechanical and chemical properties. These properties include, but are not limited to, high impact (even at low temperatures), crack & scratch resistance, food/water contact acceptable, superior chemical & weathering resistance backed by a very low water absorption and excellent dimensional stability. PA-CX12 is the perfect nylon filament for the (semi) professional print user who is looking for the perfect combination of printability and mechanical properties.

Features:

  • High-performance industrial grade nylon
  • Strong & Flexible
  • High impact, abrasion, crack & scratch resistance
  • Superior chemical & UV resistance
  • Excellent dimensional stability
  • Low water absorption
  • Food Contact Approved
Colors: M-ABS is available from stock in 12 colors. Other colors on request

Information provided by Mitsubishi Chemical.

Vendors:
Available Properties
  • Specific Gravity, ISO 1183
  • Moisture Absorption, ISO 62
  • Filament Diameter, Tolerance: 50 µm, =95% Roundness
  • Filament Diameter, Tolerance: 100 µm, =95% Roundness
  • Melt Flow, ISO 1133
  • Storage Temperature
  • Hardness, Shore D, ISO 868
  • Tensile Strength, Yield, ISO 527
  • Elongation at Break, ISO 527
  • Elongation at Yield, ISO 527
  • Tensile Modulus, ISO 527, (E)
  • Charpy Impact, Notched, ISO 179
  • Melting Point, ISO 11357
  • Vicat Softening Point, ISO 306 B
  • Processing Temperature, Printing Temperature
  • Drying Temperature
  • Dry Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.