MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Rogers Corporation Bisco® BF-2000 Ultra-Soft Silicone Foam
Categories: Polymer; Thermoset; Silicone; Silicone Foam

Material Notes: BISCO® Ultra Soft is a highly compressible silicone foam. The combination of low weight and softness makes this flame retardant foam ideal for transportation, industrial and electronics applications where low closure force and dust sealing are critical. Available in various thicknesses and manufactured in roll form.

Features and Benefits:

  • Ultra low softness allows designers to use less force to seal enclosures and still protect their device from the environment.
  • High compressibility allows material to conform to variable width gaps, thereby allowing more design flexibility.
  • Excellent memory and low stress relaxation reduces maintenance costs associated with gasket failures due to compression set and softening.
  • Resistance to ultraviolet light, ozone, extreme temperatures and flame enables consistent performance in all environments.
  • Color: black
  • Thickness: 0.125 in to 0.500 in
  • Standard Width: 0.500 in to 36.0 in

Applications:

  • Vibration isolation in electronic components and transportation vehicles
  • Low closure force gaskets within portable electronics such as laptops and LCD screens within aircraft and rail interiors
  • Fire retardant thermal insulation

Information provided by Rogers Corporation.

Vendors:
Available Properties
  • Density, ASTM D1056
  • Thickness, Range of Thicknesses Available
  • Tensile Strength, ASTM D412
  • Elongation at Break, ASTM D412
  • Compressive Yield Strength, ASTM D1056
  • Compression Set, ASTM D1056
  • Compression Set, ASTM D1056
  • Flammability, UL94, also HF-1
  • Flame Spread Index, ASTM E162, Is
  • Smoke Density, ASTM E662, <20; Ds
  • Smoke Density, ASTM E662, <50; Ds
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.