MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
SABIC LEXAN™ FR 945 PC (Asia)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LEXAN 945 Polycarbonate (PC) is an injection moldable non-chlorinated and non-brominated, unfilled flame retardant grade with medium flow. It has an MVR of 10 (300°C/1.2kg) and a UL94 V0@1.0mm, 5VA at 3.0mm rating and is available in various opaque color options.

Information provided by SABIC

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Water Absorption, ASTM D570, 24 hours
  • Moisture Absorption, ASTM D570, 50% RH, 24 hrs
  • Moisture Absorption at Equilibrium, ASTM D570
  • Linear Mold Shrinkage, Flow, SABIC method
  • Melt Flow, ASTM D1238
  • Hardness, Rockwell M, ASTM D785
  • Hardness, Rockwell R, ASTM D785
  • Tensile Strength at Break, ASTM D638, 50 mm/min
  • Tensile Strength, Yield, ASTM D638, 50 mm/min
  • Elongation at Break, ASTM D638, 50 mm/min
  • Elongation at Yield, ASTM D638, 50 mm/min
  • Tensile Modulus, ASTM D638, 50 mm/min
  • Flexural Yield Strength, ASTM D790, 1.3 mm/min, 50 mm span
  • Flexural Modulus, ASTM D790, 1.3 mm/min, 50 mm span
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Unnotched, ASTM D4812
  • Dart Drop, Total Energy, ASTM D3763
  • Arc Resistance, ASTM D495
  • Comparative Tracking Index, UL 746A
  • Hot Wire Ignition, HWI, UL 746A
  • High Amp Arc Ignition, HAI, UL 746A
  • High Voltage Arc-Tracking Rate, HVTR, UL 746A
  • CTE, linear, Parallel to Flow, ASTM E831
  • CTE, linear, Transverse to Flow, ASTM E831
  • Specific Heat Capacity, ASTM C 351
  • Thermal Conductivity, ASTM C177
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648, unannealed
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, unannealed
  • Vicat Softening Point, ASTM D1525, Rate B/50
  • UL RTI, Electrical, UL 746B
  • UL RTI, Mechanical with Impact, UL 746B
  • UL RTI, Mechanical without Impact, UL 746B
  • Flammability, UL94, UL 94
  • Flammability, UL94, UL 94
  • Flammability, UL94, UL 94
  • Oxygen Index, ISO 4589
  • Glow Wire Test, IEC 60695-2-12
  • Glow Wire Test, IEC 60695-2-13
  • Glow Wire Test, IEC 60695-2-12
  • Nozzle Temperature, Injection Molding
  • Zone 1
  • Zone 2
  • Zone 3
  • Melt Temperature
  • Mold Temperature
  • Drying Temperature, Injection Molding
  • Dry Time, Injection Molding
  • Dry Time, Cumulative; Injection Molding
  • Moisture Content
  • Back Pressure
  • Shot Size
  • Vent Depth
  • Screw Speed
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Saudi Basic Industries Corporation; SABIC Innovative Plastics (GE Plastics)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.