MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Poly-u-Mac Air-Comb PP8-80 Polypropylene Honeycomb Material
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Air-Comb PP8-80 is a polypropylene honeycomb material that combines lightweight, strength and resilience. It is suitable for a wide variety of sandwich core applications in marine, road/ rail transportation, industry and infrastructure. Air-Comb also possesses excellent sound damping properties. Air-Comb is available in plain, contoured, and double contoured finishes and comes standard with a non-woven veil and barrier film. Air-Comb is also available without the veil and barrier film by special order. Poly-U-Mac is able to supply Air-Comb in ready-to-use kits. Designed to be used straight out of the box. Poly-U-Mac Air-Comb kits save labor costs, speed the manufacturing process and virtually eliminate material waste.

Key Features & Benefits:

  • High strength to weight ratio
  • Excellent sound dampening properties
  • Resistance to corrosion, rot and moisture
  • Wide temperature range (-22 to 176°F)
  • Recyclable
Typical Applications:
  • Leisure & Commercial Marine: decks, bulkheads, stringers & transoms
  • Road Transportation: cabs, sleeper floors, trailer beds & walls
  • Rail Transportation: floors, driver's cabs, exterior & interior paneling
  • Industry: exhibition displays, bathtubs & shower floors
  • Infrastructure: portable buildings, claddings & interior paneling

    Information provided by Poly-u-Mac

Vendors:
Available Properties
  • Density
  • Compressive Strength
  • Shear Strength
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.