MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
Hardwire 3S-23-12 High Density Composite
Categories: Metal; Ferrous Metal; Carbon Steel; High Carbon Steel; Metal Foam, Mesh, or Honeycomb

Material Notes: The 3S Hardwire is a high carbon steel cord with a micro-fine brass or AO-brass (Adhesion Optimized) coating. The 3S cord is used where balanced compressive and tensile strengths are required and represents the ultimate in economical value when measured in modulus per dollar. The 3S wire cord is made by twisting three identical wire filaments (All filaments are 0.0189 in diameter) together at a longer than usual lay length. The result is a cord with lower twist angles and straighter filaments that is the basis for the increased compressive strengths.

Characteristics:

  • 3S tapes have the highest compressive strengths of all Hardwire tapes and tend to match or exceed the tensile properties.
  • Best value for stiffness per dollar as well as flexural and compressive strengths per dollar.
  • The cords do not bloom in failure modes during compression or tension.
  • Laminates exhibit steel like characteristics with high ductility and extreme deflection capability.
  • Very high flexural strength as well as ductile failure modes (laminates tend to bend – not break).
  • Tapes bend very easily and uniformly in standard sheet metal breaks.
  • It is the boardiest of all Hardwire tapes – excellent for flat surfaces but still conformable enough for curved structures.

All information provided by Hardwire, LLC.

Vendors:
Available Properties
  • Density, Laminate Density
  • Modulus of Elasticity, Effective Modulus
  • Flexural Yield Strength, Sheet Stress
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Hardwire, LLC

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2026 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.