MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Kohesi Bond KB-SS-MOD One component, electrically insulative sodium silicate based system
Categories: Ceramic; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Product Highlights:
  • Superb electrical insulation
  • Very cost effective
  • Good flow properties
  • Resists more than 815°C
  • Effective moisture barrier
  • Ease of application
Kohesi Bond KB-SS-MOD is a modified, aqueous sodium silicate based system for bonding and coating. This product offers very good high temperature resistance. KB-SS-MOD has a wide service temperature range of -18°C to +815°C. This product can be easily applied with a brush or a spraying system. It can cure at room temperature in 1-2 days or it can be heat cured at 80°C for 1-2 hours. However, it is recommended to cure the product at 90°C for 30 minutes followed by an additional cure at 150°C for 30 minutes. To avoid the system from causing “blistering”, special care should be taken to slowly ramp the curing temperature over a 15-30 minute span. KB-SS-MOD offers outstanding optical clarity, especially in the range of 200nm - 350nm. This colorless system is non-toxic, non-flammable and odorless. It attains most of its strength and temperature resistance properties at 70%-90% of full cure. At this point, the adhesive can be removed by exposing it to boiling water for a few hours. However, KB-SS-MOD can withstand boiling water upon achieving a full cure. This product is highly alkaline and can affect substrates like glass. It offers very good flow properties, dimensional stability and excellent electrical insulation properties. It can adhere to a wide variety of substrates, such as metals, ceramics, composites and many plastics. KB-SS-MOD is a specialized system formulated for use in aerospace, electronics, optical and specialty OEM applications requiring better strength.

Typical Applications:

  • Bonding
  • Coating

Information provided by Kohesi Bond Custom Engineered Adhesives

Vendors:
Available Properties
  • Density
  • Solids Content
  • pH
  • Viscosity
  • Tensile Strength
  • Volume Resistivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time, Optimum Cure: 30 min at 90°C followed by 30 min 150°C
  • Cure Time, Option 2
  • Cure Time, Option 1
  • Shelf Life, in original unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.