MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
Universal Wire Works No. 21 Cobalt Alloy Welding Wire
Categories: Metal; Nonferrous Metal; Cobalt Alloy; Superalloy

Material Notes: Universal No. 21 is a cobalt-chromium-molybdenum alloy designed for covered electrode, TIG, MIG, hard surfacing applications. The work-hardening characteristics, high ductility properties, excellent resistance to impact and metal to metal wear suit Universal 21 to severe applications where a work-hardening material is desired (as welded Rc 20; work hardened Rc 40 - 43).

Universal 21 applications include: high temperature valves, high pressure valves, hot punches crushing knives, drop forging dies, tap hole augers, pump shafts and sleeves, press dies, vapor tight valve seats.

Alloy 21 work hardens in service, has excellent erosion, corrosion and metal to metal wear resistance. Deposits exhibit effective hardness and a good cutting edge at high temperatures. On thick overlays Alloy 21 can be used as a buildup prior to depositing a higher hardness alloy.

Machinability: Use carbide tools.

Information provided by Universal Wire Works for their line of welding wire and filler metal.

Vendors:
Available Properties
  • Hardness, Rockwell C, As Welded
  • Hardness, Rockwell C, Work Hardened
  • Tensile Strength, Ultimate
  • Melting Point
  • Carbon, C
  • Chromium, Cr
  • Cobalt, Co, As remainder
  • Iron, Fe
  • Molybdenum, Mo
  • Nickel, Ni
  • Silicon, Si
  • Tungsten, W
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.