MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
Arla SAPHIR® AS PC Sheet
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Extruded

Material Notes: SAPHIR® is a range of polycarbonate coated sheet. SAPHIR® AS, is an antistatic coated polycarbonate sheet with a unique protection against electrostatic charging. SAPHIR® AS is a polycarbonate sheet with a two side anti-static coating. The coating gives an effective protection against electrostatic charging and prevents dust and dirt attraction. SAPHIR® AS prevents electrostatic discharge (ESD) and the high impact strength of polycarbonate is combined with excellent fire properties and optical clarity. SAPHIR® AS is to be used in flat applications.

Benefits: Protection against electrostatic charging; Prevent dust and dirt attraction; Impact Resistant; More than 10 times the impact strength of high impact PMMA

Application: SAPHIR® AS is suitable for hoods and inspection glazing for testing equipment. In applications where it is important to prevent electrostatic build up, such as explosive atmospheres.

Information provided by Arla Plast.

Vendors:
Available Properties
  • Density, ISO 1183
  • Moisture Absorption, ISO 62, 50% RH
  • Tensile Strength at Break, ISO 527
  • Tensile Strength, Yield, ISO 527
  • Elongation at Break, ISO 527
  • Elongation at Yield, ISO 527
  • Modulus of Elasticity, ISO 527
  • Flexural Modulus, ISO 178
  • Izod Impact, Notched (ISO), ISO 180/1A
  • Izod Impact, Notched (ISO), ISO 180/1A
  • Charpy Impact Unnotched, ISO 179/1eU
  • Charpy Impact, Notched, ISO 179/1eA
  • Surface Resistance, ASTM D257
  • CTE, linear, ISO 11359-2
  • Thermal Conductivity, DIN 8302
  • Refractive Index, ISO 489
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.