MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Eastman Pamolyn™ 125 Oleic Acid
Categories: Fluid

Material Notes: Product Description: Pamolyn™ 125 oleic acid is a high purity, commercial grade oleic acid derived wholly from a tall oil fatty acid source. It is a low odor, pale, color stable, low titer, oily liquid. Compared with commercial grades from other vegetable or animal sources, Pamolyn™ 125 oleic acid is high in oleic acid and low in saturated acid content. Unlike tallow source oleic acids, it is free of lower molecular weight acids. All fatty acids in Pamolyn™ 125 oleic acid are of C18 origin. Pamolyn™ 125 oleic acid is designed for a broad range of applications. Typical uses, when it is converted to soaps, sulfonated products, and other derivatives, include: textile processing aids, automotive additives and mold lubricants, agents for production of synthetic rubber, and surfactants for a variety of other uses.

Application/Uses:

  • Building and Construction
  • Hot Melt Adhesives
  • Lubricants
  • Paint and Coatings
  • Personal Care and Cosmetics
  • Solventborne Adhesives
Key Attributes:
  • Excellent color stability
  • High oleic acid content
  • Low odor level & uniform fatty acid composition
  • Low saturated acids and unsaponifiables content
  • Pale initial color

Information provided by Eastman

Vendors:
Available Properties
  • Density
  • Total Acid Number
  • Gardner Color Number
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Eastman Chemical Company

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.