MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.
Wacker Silpuran® 6740/40 A/B Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Product description: SILPURAN® 6740/40 A/B is a paste-like, easily-pigmentable two-component liquid silicone rubber compound with short curing time. Vulcanizates are noted for their self-adhesive properties to various substrates and excellent mechanical properties.

Special features: SILPURAN® 6740/40 A/B meets selected test requirements of ISO 10993 and United States Pharmacopoeia (USP) Class VI. Postcured parts can be used for food contact applications and are suitable for use under the Recommendation "XV. Silicones" of the BfR and FDA § 177.2600 under observance of any given limitations on extractable and volatile substances. SILPURAN® 6740/40 A/B is a primerless self-bonding grade that adheres to various substrates. The bonding is improved by an ageing process (e.g. one hour at 100°C) or by a longer storage at room temperature. Because of the individual surface properties each substrate must be tested before mass production. If nesserary one has to check the development of adhesive properties over time and/or in an environment relevant to the application.

Application: This grade is particularly suitable for the economical production of large series of injection molded articles. SILPURAN® 6740/40 A/B is designed for medical applications including implantation for < 30 days.

Information provided by Wacker Chemie AG.

Vendors:
Available Properties
  • Density, DIN EN ISO 1183-1 A
  • Viscosity, DIN 53019
  • Viscosity, DIN 53019
  • Hardness, Shore A, DIN 53505
  • Tensile Strength at Break, DIN 53505 S1
  • Elongation at Break, DIN 53505 S1
  • Tear Strength, ASTM D624B
  • Transmission, Visible, "Transparent" but manufacturer does not quantify.
  • Cure Time
  • USP Class VI
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

USP Class VI adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.