MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.
Lucas-Milhaupt SILVALOY® 071 (BRAZE™ 071, SILVALOY® B7T) Copper Silver Tin Brazing Filler Metal
Categories: Metal; Nonferrous Metal; Copper Alloy; Solder/Braze Alloy

Material Notes: Silvaloy 071 flows well on steels, without the use of flux, in controlled atmosphere furnace brazing. It can be used in place of copper brazing in many applications. Silvaloy 071 has also been used where a high temperature brazing alloy is required because it is desired to heat-treat steel after brazing. The small degree of melting that occurs in Silvaloy 071 at 1225°F does not appear to interfere with such applications. Silvaloy 071 is a low cost, high temperature silver brazing filler metal with an extremely long (580°F) melting range. Generally, it is not recommended for torch brazing but flows well on carbon steels, without flux, when used in a reducing furnace atmosphere.

Available forms: Wire, strip, engineered preforms, specialty preforms.

Information provided by Lucas-Milhaupt.

Vendors:
Available Properties
  • Specific Gravity
  • Density
  • Electrical Resistivity, 12.8% IACS
  • Melting Point
  • Solidus
  • Liquidus
  • Processing Temperature, Brazing Range
  • Copper, Cu
  • Other, total
  • Silver, Ag
  • Tin, Sn
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

solder replacement adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.