MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Geon® Performance Solutions 130 Series 137 Polyvinyl Chloride Copolymer (PVC Copolymer)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Geon® 137 is a carboxyl functional copolymer dispersion resin providing extra adhesion to synthetic fabrics, such as nylon, allowing the elimination of adhesion promoters. It provides the ability to crosslink with epoxies, providing a more solvent resistant coating. The polarity of Geon® 137 allows its use in hydrosols. Geon® 137 is recommended for applications where special characteristics are requires, such as nylon fabric coating, hydrosol inks and coatings, solvent resistant coatings, and automotive sealants.

Note: The value set forth represent typical values and PolyOne Corporation, therefore, makes no representation that the material in any particular shipment will conform to the listed properties. Packaging: This resin is shipped in multi-wall paper bags, net weight 50 lbs, 2500 lbs per pallet. Information shown on the package includes commercial identification number, lot and weight. Geon® ALTC and ASTM D638 (formulation): 100phr Geon® 137, 77phr DINP, 3phr ESO, and 2phr Therm-Chek SP 120 LOHF Geon® STP 390(formulation): 100phr Geon® 137, and 60phr DOP

Geon Performance Solutions was created from PolyOne in 2019.

Vendors:
Available Properties
  • Specific Gravity
  • Bulk Density
  • Fineness, Hegman, North Fineness; Geon® 390
  • Relative Viscosity, Internal Method, Correlation, Cyclohexanone 1%
  • Brookfield Viscosity, Internal Method, Initial Viscosity @ 2 rpm; Geon® ALTC 22 (with provided formulation)
  • Brookfield Viscosity, Internal Method, One Day Viscosity @ 2 rpm; Geon® ALTC 22 (with provided formulation)
  • Brookfield Viscosity, Internal Method, Initial Viscosity @ 20 rpm; Geon® ALTC 22 (with provided formulation)
  • Brookfield Viscosity, Internal Method, One Day Viscosity @ 20 rpm; Geon® ALTC 22 (with provided formulation)
  • Viscosity Measurement, ASTM D1243-60-A, Inherent
  • Melt Flow, Internal Method, Severs Efflux; Geon® ALTC 23 (with provided formulation)
  • Tensile Strength, ASTM D638, Optimum; With provided formulation
  • Gloss, Internal Method, 60 Degree Fused 5 mins @ 350 F Geon® ALTC 65 (with provided formulation)
  • Transmission, Visible, Internal Method, Geon® ALTC 66 (with provided formulation)
  • Moisture Content, Internal Method, Karl FisherGeon® STP 683
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.