MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Shandong Dongyue Shenzhou New Material Co CHF110 Perfluorosulfonic Acid Ion-Exchange Resin (PFSA)
Categories: Polymer; Thermoplastic; Fluoropolymer

Material Notes: Conformable with: Q/DYS 001-2007

Perfluorosulfonic Acid Ion-Exchange Resin is a polymer, with good stability and chemical resistance properties, which are widely used in chlor-alkali industry, proton exchange membrane fuel cells, lithium-ion rechargeable batteries, other fields such as electrolysis devices, sewage disposal, chemical catalysis, photocatalysis, gas separation, functional composite materials, particular electrical active polymers used for robot.

Main Applications:

The resin can be used to produce ion exchange conductive membrane, fuel cell proton ion membrane, super acid catalyst, super stable ion-exchange agent, etc.

Information Provided by Shandong Dongyue Shenzhou New Material Co., Ltd.

Vendors:
Available Properties
  • Density, Resin
  • Decomposition Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.