MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Plaslok 5440 Black General Purpose Phenolic Molding Compound  (discontinued **)
Categories: Polymer; Thermoset; Phenolic

Material Notes: Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.

Plaslok 5440 is the replacement material for the former Union Carbide BMRS-5440. It is a two-stage, phenolic molding compound that has been successfully formulated to accommodate a very wide range of molding situations. Because of its balance of physical and electrical properties it has found use in a variety of applications including knobs, circuit breaker cases and wiring devices.

Data provided by Plaslok Corporation.

Vendors:
Available Properties
  • Density, ASTM D792
  • Apparent Bulk Density, ASTM D1895
  • Water Absorption, ASTM D570
  • Linear Mold Shrinkage, Compression; ASTM D955
  • Tensile Strength, Ultimate, ASTM D638
  • Flexural Yield Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Compressive Yield Strength, ASTM D695
  • Electrical Resistivity, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149
  • Dissipation Factor, ASTM D150
  • Dissipation Factor, ASTM D150
  • Comparative Tracking Index, UL 746
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • UL RTI, Electrical
  • UL RTI, Mechanical with Impact
  • UL RTI, Mechanical without Impact
  • Flammability, UL94
  • Flammability, UL94
  • Oxygen Index, ASTM D2863
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Plenco (Former Plaslok Product)

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.