MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
DuPont Mobility and Materials Kalrez® PV8070 Fluoroelastomer  (discontinued **)
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: DuPont™ Kalrez® PV8070 perfluoroelastomer parts are a black product for PV cell manufacturing processes requiring high temperature resistance including doping for n-type layer formation (bulk c-Si), diffusion for diselenide thermal implantation (CGIS) and TCS-based thermal CVD for poly-silicon feedstock production. It exhibits outstanding thermal stability and has excellent (low) compression set and outgassing properties. It also offers excellent resistance to both chlorine and fluorine gas as well as other dry process chemistry. Kalrez® PV8070 perfluoroelastomer parts have excellent mechanical strength properties and are well suited for both static and dynamic sealing applications. A maximum continuous service temperature of 325 °C is suggested. Short excursions to higher temperatures may also be possible.

Features/Benefits

  • Outstanding thermal stability
  • Excellent (low) compression set and outgassing properties
  • Excellent resistance to dry process chemistry
  • Excellent mechanical strength properties

    Suggested Applications

    • Chamber lid and door seals
    • Center ring seals and fittings
    • Isolation valve seals
    • Quartz tube seals
    • Substrate handling pads

Vendors:
Available Properties
  • Hardness, Shore M, ASTM D1414, ASTM D2240
  • Compression Set, ASTM D1414 and ASTM D395B
  • Compression Set, ASTM D1414 and ASTM D395B
  • Maximum Service Temperature, Air, DuPont Test Method
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
DuPont Performance Polymers (Former DuPont Elastomers)

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.